CP GRADE 12

Common Name
Titanium Grade 12
Ti-CODE 12™
Ti-0.3Mo-0.8Ni
UNS
R53400
General Information
“Titanium Alloy Grade 12 is lightly alloyed near-alpha alloy offering improved strength at elevated temperatures and optimum ASME Code design allowables. The material is readily weldable, and has superior crevice corrosion resistance. This material is very corrosion resistant in highly oxidizing and mildly reducing environments. The alloy is available as wire, plate, sheet, strip, forgings, bar, and billet.”
Common Specification
Specification Product Form
AMS 4902
ASME B861 (Grade 12)* Seamless Pipe
ASME B862 (Grade 12)* Welded Pipe
ASME SB-381 Forgings
ASME SB-348 Bars and Billets
ASTM B265 (Grade 12) Sheet, Strip and Plate
ASTM B338
ASTM B348 (Grade 12) Bars and Billets
ASTM B337 (Grade 12) Welded and Seamless Pipe
ASTM B381 (Grade 12) Forgings
ASTM B861
ASTM B862
AWS A5.16 (ERTi-12) Weld Wire

*replacing ASTM B337

Chemistry Requirements
N C >H Fe O Mo Ni Residual Each Max Residuals Max Total Ti
0.03 0.1 0.015 0.3 0.4 0.2-0.4 0.6-0.9 0.1 0.4 Balance

% Maximum unless given as a range.

Minimum Tensile Properties
Condition UTS ksi (Mpa) >0.2%YS ksi (MPA) % El. % RA*
As specified (shape) 70 (483) 50 (345) 18 25
Minimum Tensile Properties
Condition UTS ksi (Mpa) >0.2%YS ksi (MPA) % El. % RA*
As specified (shape) 70 (483) 50 (345) 18 25

Note: Typical properties are not to be utilized as a requirement, but are only listed for guidance. These properties may or may not be attainable in all circumstances.
* %Ra not required by all specifications
 
Trademark Notice: Some names are trade names and/or trademarks of specific manufacturers. Titan Singapore is not affiliated with any manufacturer(s). Orders will be filled to meet specifications from any available source(s). Names are listed solely for reference to help identify products consistent with listed specifications.

CP GRADE 12