CP GRADE 17
Common Name | |
---|---|
CP Grade 17 | CP Grade 17 |
Titanium Grade 17 | Titanium Grade 17 |
UNS | |
R52252 | |
General Information | |
Titanium Alloy Grade 17 is “alloyed” titanium offering optimum ductility and cold formability, with properties similar to Grade 1 and Grade 11. Grade 17 is like Grade 11 but with lower palladium. The material is readily weldable. This material is very corrosion resistant in highly oxidizing and mildly reducing environments. The material is castable and may be utilized in cast valves and fittings. The alloy is available as castings, wire, welded tube, pipe, plate, sheet, strip, forgings, bar, and billet. | |
Common Specification | |
Specification | Product Form |
ASTM B265 (Grade 17) | Strip, Sheet and Plate |
ASTM B348 (Grade 17) | Bar and Billet |
ASTM B367 (Grade 17) | Castings |
ASTM B381 (Grade 17) | Forgings |
Chemistry Requirements | ||||||||
---|---|---|---|---|---|---|---|---|
N | C | >H | Fe | O | Pd | Residual Each Max | Residuals Max Total | Ti |
0.03 | 0.08 | 0.015 | 0.20 | 0.18 | 0.04-0.08 | 0.1 | 0.4 | Balance |
% Maximum unless given as a range.
Minimum Tensile Properties | ||||
---|---|---|---|---|
Condition | UTS ksi (Mpa) | >0.2%YS ksi (MPA) | % El. | % RA* |
As specified (shape) | 35 (240) | 25 (170) | 24 | 30 |
Typical Tensile Properties | ||||
---|---|---|---|---|
Condition | UTS ksi (Mpa) | >0.2%YS ksi (MPA) | % El. | % RA* |
As provided | 50 (345) | 34 (221) | 37 | – |
Note: Typical properties are not to be utilized as a requirement, but are only listed for guidance. These properties may or may not be attainable in all circumstances.
* %Ra not required by all specifications
Trademark Notice: Some names are trade names and/or trademarks of specific manufacturers. Titan Singapore is not affiliated with any manufacturer(s). Orders will be filled to meet specifications from any available source(s). Names are listed solely for reference to help identify products consistent with listed specifications.